Nylon 6 30% Glass Filled Technical Data
Property |
Test
Method
|
Units
|
UNIPA
MRg
|
|
|
|
30% Glass
Fiber Filled Nylon 6
|
Mechanical
|
Specific
Gravity |
ASTM-D792
|
---
|
1.28
|
Tensile
Strength |
ASTM-D638
|
psi
|
18,000
|
Tensile
Elongation |
ASTM-D638
|
%
|
8
|
Tensile
Modulus of Elasticity |
ASTM-D638
|
psi
|
|
Flexural
Strength |
ASTM-D790
|
psi
|
25,000
|
Flexural
Modulus of Elasticity |
ASTM-D790
|
psi
|
|
Compressive
Strength |
ASTM-D695
|
psi
|
25,000
|
Izod
Notched Impact |
ASTM-D256
|
ft.-lb./in.
|
1.0
|
Rockwell
Hardness |
ASTM-D785
|
M or R
scale
|
M100
|
Thermal |
Coef.
of Linear Thermal Expansion |
ASTM-D696
|
in./in./deg
F
|
1.5
x 10-5 |
Max.
Continuous Use Temp. |
Nytef
std.
|
F
|
210
|
Heat
Deflection Temp. @ 264 psi
|
ASTM-D648
|
F
|
300
|
Melting
Point |
ASTM-D3418
|
F
|
430
|
Electrical |
Dielectric
Strength-Short Term |
ASTM-D149
|
volts/mil
|
500
|
Dielectric
Constant @ 106 Hz |
ASTM-D150
|
|
3.7
|
Dissipation
Factor @ 60 Hz |
ASTM-D150
|
|
.02
|
Volume
Resistivity |
ASTM-D257
|
ohm-cm
|
>1013
|
Miscellaneous |
Water
Absorption/24 hrs. |
ASTM-D570
|
% weight
|
0.4
|
Water
Absorption @ Saturation |
ASTM-D570
|
% weight
|
3.5
|
Flammability |
UL-94
|
|
HB
|
Dynamic
Coefficient of Friction
|
|
|
0.33
|
Agency
Approvals |
FDA/USDA |
|
|
No
|
3-A
Dairy |
|
|
No
|
|
|